Rolling-Contact Fatigue Studies With Four Tool Steels and a Crystallized Glass Ceramic

[+] Author and Article Information
Erwin V. Zaretsky, William J. Anderson

Lewis Research Center, NASA, Cleveland, Ohio

J. Basic Eng 83(4), 603-610 (Dec 01, 1961) (8 pages) doi:10.1115/1.3662277 History: Received December 20, 1960; Online November 04, 2011

Abstract

The rolling-contact fatigue properties of crystallized glass ceramic balls together with AISI M-1, AISI M-50, Halmo, and WB-49 alloy steel balls tempered to various hardness levels were determined in the NASA spin rig and in the five-ball fatigue tester. A continuous increase in fatigue life and load capacity for each steel was observed with increased ball hardness. These results correlate with resistance to plastic deformation as measured with spherical specimens in rolling contact but do not correlate with elastic limit and yield strength measured for bar specimens. These bar specimens showed optimum values at intermediate hardness levels. Extremely low scatter in fatigue life for the ceramic balls indicate that the degree of structural homogeneity may be an important factor in life scatter of bearing materials.

Copyright © 1961 by ASME
Your Session has timed out. Please sign back in to continue.

References

Figures

Tables

Errata

Discussions

Some tools below are only available to our subscribers or users with an online account.

Related Content

Customize your page view by dragging and repositioning the boxes below.

Related Journal Articles
Related eBook Content
Topic Collections

Sorry! You do not have access to this content. For assistance or to subscribe, please contact us:

  • TELEPHONE: 1-800-843-2763 (Toll-free in the USA)
  • EMAIL: asmedigitalcollection@asme.org
Sign In