This paper describes an experimental analysis of a planar solid oxide fuel cell (SOFC) single unit cell with Crofer22APU plate assembly. The work reports the electrical behavior of such a system by outlining the time-evolution of contact resistances between the air electrode and the stainless steel plate. Moreover, the stability and effectiveness of a glass-ceramic sealant used to join Crofer22APU interconnector to an anode supported cell is also discussed. The time-evolution of the open circuit voltage was investigated with respect to the eventual sealant degradation or chromium poisoning issues by the metallic interconnector; a rapid voltage degradation at open circuit voltage was measured after 150 h. Chromium poisoning was found to degrade the fuel cell performance, whereas the sealant was chemically and physically stable, as shown by a post-mortem analysis on the cell components.

1.
Akbay
,
T.
,
Chitose
,
N.
,
Miyazawa
,
T.
,
Shibata
,
M.
,
Nishiwaki
,
F.
, and
Inagaki
,
T.
, 2009, “
Computational Fluid Dynamic Analysis of a Seal-Less Solid Oxide Fuel Cell Stack
,”
ASME J. Fuel Cell Sci. Technol.
1550-624X,
6
, p.
041007
.
2.
Haberman
,
B. A.
, and
Young
,
J. B.
, 2008, “
A Detailed Three-Dimensional Simulation of an IP-SOFC Stack
,”
ASME J. Fuel Cell Sci. Technol.
1550-624X,
5
, p.
011006
.
3.
Shimada
,
T.
,
Kato
,
T.
, and
Tanaka
,
Y.
, 2007, “
Numerical Analysis of Thermal Behavior of Small Solid Oxide Fuel Cell Systems
,”
ASME J. Fuel Cell Sci. Technol.
1550-624X,
4
, pp.
299
307
.
4.
Kornely
,
M.
,
Neumann
,
A.
,
Menzler
,
N. H.
, and
Ivers-Tiffée
,
E.
, 2010, “
Degradation of ASC Performance by Cr-Poisoning
,”
Proceedings of the Ninth European Solid Oxide Fuel Cell Forum
, Jun. 29–Jul. 2, Lucerne, Switzerland.
5.
Bae
,
J.
, 2007, “
Small Stack Performance of Intermediate Temperature-Operating Solid Oxide Fuel Cells Using Stainless Steel Interconnects and Anode-Supported Single Cell
,”
J. Power Sources
0378-7753,
172
, pp.
100
107
.
6.
Jiang
,
S. P.
, and
Zhen
,
Y.
, 2008, “
Mechanism of Cr Deposition and Its Application in the Development of Cr-Tolerant Cathodes of Solid Oxide Fuel Cells
,”
Solid State Ionics
0167-2738,
179
, pp.
1459
1464
.
7.
Blum
,
L.
,
Gross
,
S.
,
Malzbender
,
J.
,
Pabst
,
U.
,
Peksen
,
M.
,
Peters
,
R.
, and
Vinke
,
I. C.
, “
Investigation of SOFC Sealing Behaviour Under Stack Relevant Conditions at Forschungszentrum Jülich
,”
J. Power Sources
0378-7753, in press.
8.
Chou
,
Y. S.
,
Stevenson
,
J. W.
, and
Singh
,
P.
, 2005, “
Thermal Cycle Stability of a Novel Glass–Mica Composite Seal for Solid Oxide Fuel Cells: Effect of Glass Volume Fraction and Stresses
,”
J. Power Sources
0378-7753,
152
, pp.
168
174
.
9.
Chung
,
D. Y.
,
Heo
,
Y. H.
,
Lee
,
S. B.
,
Lim
,
T. H.
,
Song
,
R. H.
, and
Shin
,
D. R.
, “
Induction Brazing for Gas Sealing of Anode-Supported Tubular Solid Oxide Fuel Cells Using the Nickel Based Brazing Alloy Modified by TiH2
,”
Int. J. Hydrogen Energy
0360-3199, in press.
10.
Miguel-Pérez
,
V.
,
Martínez-Amesti
,
A.
,
Vidal
,
K.
,
Larrañaga
,
A.
,
,
M. L.
, and
Arriortua
,
M. I.
, 2010, “
Oxidation Study of Different Metallic Interconnects in SOFC Application
,”
Proceedings of the Ninth European Solid Oxide Fuel Cell Forum
, Jun. 29–Jul. 2, Lucerne, Switzerland.
11.
Morel
,
B.
,
Oresic
,
B.
, and
Reytier
,
M.
, 2010, “
Experimental Study of Mechanical Load Effects on Contact Resistance Between Interconnectors and Electrodes in SOFC or HTSE Stacks
,”
Proceedings of the Ninth European Solid Oxide Fuel Cell Forum
, Jun. 29–Jul. 2, Lucerne, Switzerland.
12.
Jiang
,
S. P.
,
Zhang
,
J. P.
, and
Zheng
,
X. G.
, 2002, “
A Comparative Investigation of Chromium Deposition at Air Electrodes of Solid Oxide Fuel Cell
,”
J. Eur. Ceram. Soc.
0955-2219,
22
, pp.
361
373
.
13.
Lee
,
S.
,
Chu
,
C. -L.
,
Tsai
,
M. -J.
, and
Lee
,
J.
, 2010, “
High Temperature Oxidation Behavior of Interconnect Coated With LSCF and LSM for Solid Oxide Fuel Cell by Screen Printing
,”
Appl. Surf. Sci.
0169-4332,
256
, pp.
1817
1824
.
14.
Sugita
,
S.
,
Yoshida
,
Y.
,
Orui
,
H.
,
Nozawa
,
K.
,
Arakawa
,
M.
, and
Arai
,
H.
, 2008, “
Cathode Contact Optimization and Performance Evaluation of Intermediate Temperature-Operating Solid Oxide Fuel Cell Stacks Based on Anode-Supported Planar Cells With LaNi0.6Fe0.4O3 Cathode
,”
J. Power Sources
0378-7753,
185
, pp.
932
936
.
15.
Megel
,
S.
,
Girdauskaite
,
E.
,
Sauchuk
,
V.
,
Kusnezoff
,
M.
, and
Michaelis
,
A.
, 2010, “
Area Specific Resistance of Oxide Scales Grown on Ferritic Alloys for Solid Oxide Fuel Cell Interconnects
,”
Proceedings of the Ninth European Solid Oxide Fuel Cell Forum
, Jun. 29–Jul. 2, Lucerne, Switzerland.
16.
Singh
,
R. N.
, 2007, “
Sealing Technology for Solid Oxide Fuel Cells (SOFC)
,”
Int. J. Appl. Ceram. Technol.
1546-542X,
4
, pp.
134
144
.
17.
Fergus
,
J. W.
, 2005, “
Sealants for Solid Oxide Fuel Cells
,”
J. Power Sources
0378-7753,
147
, pp.
46
57
.
18.
Mahapatra
,
M. K.
, and
Lu
,
K.
, 2010, “
Glass-Based Seals for Solid Oxide Fuel and Electrolyzer Cells—A Review
,”
Mater. Sci. Eng. R.
0927-796X,
67
, pp.
65
85
.
19.
Chou
,
Y. -S.
,
Stevenson
,
J.
, and
Gow
,
R. N.
, 2007, “
Novel Alkaline Earth Silicate Sealing Glass for SOFC. Part I. The Effect of Nickel Oxide on the Thermal and Mechanical Properties
,”
J. Power Sources
0378-7753,
168
, pp.
426
433
.
20.
Singh
,
R. N.
, 2006, “
High Temperature Seals for Solid Oxide Fuel Cells
,”
J. Mater. Eng. Perform.
1059-9495,
15
, pp.
422
426
.
21.
Tucker
,
M. C.
,
Jacobson
,
C. P.
,
De Jonghe
,
L. C.
, and
Visco
,
S. J.
, 2006, “
A Braze System for Sealing Metal-Supported Solid Oxide Fuel Cells
,”
J. Power Sources
0378-7753,
160
, pp.
1049
1057
.
22.
Smeacetto
,
F.
,
Salvo
,
M.
,
Ferraris
,
M.
,
Cho
,
J.
, and
Boccaccini
,
A. R.
, 2008, “
Glass–Ceramic Seal to Join Crofer22APU Alloy to YSZ Ceramic in Planar SOFCs
,”
J. Eur. Ceram. Soc.
0955-2219,
28
, pp.
61
68
.
23.
Smeacetto
,
F.
,
Salvo
,
M.
,
Ferraris
,
M.
,
Casalegno
,
V.
,
Asinari
,
P.
, and
Chrysanthou
,
A.
, 2008, “
Characterization and Performance of Glass–Ceramic Sealant to Join Metallic Interconnects to YSZ and Anode-Supported-Electrolyte in Planar SOFCs
,”
J. Eur. Ceram. Soc.
0955-2219,
28
, pp.
2521
2527
.
24.
Smeacetto
,
F.
,
Chrysanthou
,
A.
,
Salvo
,
M.
,
Zhang
,
Z.
, and
Ferraris
,
M.
, 2009, “
Performance and Testing of Glass-Ceramic Sealant Used to Join Anode-Supported-Electrolyte to Crofer22APU in Planar Solid Oxide Fuel Cells
,”
J. Power Sources
0378-7753,
190
, pp.
402
407
.
25.
Niewolak
,
L.
,
Quadakkers
,
W. J.
,
Bentzen
,
J. J.
,
Høgh
,
J. V. T.
, and
Zhang-Steenwinkel
,
Y.
, 2010, “
Overview of Results on Interconnect Steels and Coatings
,”
SOFC600 Mini Conference
, Royal Flemish Academy of Belgium for Science and the Arts, Brussels.
26.
Lanzini
,
A.
, and
Leone
,
P.
, 2010, “
Experimental Investigation of Direct Internal Reforming of Biogas in Solid Oxide Fuel Cells
,”
Int. J. Hydrogen Energy
0360-3199,
35
, pp.
2463
2476
.
27.
Leone
,
P.
,
Santarelli
,
M.
,
Asinari
,
P.
,
Calì
,
M.
, and
Borcheillini
,
R.
, 2008, “
Experimental Investigations of the Microscopic Features and Polarization Limiting Factors of Planar SOFCs With LSM and LSCF Cathodes
,”
J. Power Sources
0378-7753,
177
, pp.
111
122
.
28.
Fontana
,
S.
,
Amendola
,
R.
,
Chevalier
,
S.
,
Piccardo
,
P.
,
Caboche
,
G.
,
Viviani
,
M.
,
Molins
,
R.
, and
Sennour
,
M.
, 2007, “
Metallic Interconnects for SOFC: Characterisation of Corrosion Resistance and Conductivity Evaluation at Operating Temperature of Differently Coated Alloys
,”
J. Power Sources
0378-7753,
171
, pp.
652
662
.
29.
Fergus
,
J. W.
, 2007, “
Effect of Cathode and Electrolyte Transport Properties on Chromium Poisoning
,”
Int. J. Hydrogen Energy
0360-3199,
32
, pp.
3664
3671
.
30.
Chou
,
Y. -S.
,
Stevenson
,
J. W.
, and
Meinhardt
,
K. D.
, 2010, “
Electrical Stability of a Novel Refractory Sealing Glass in a Dual Environment for Solid Oxide Fuel Cell Applications
,”
J. Am. Ceram. Soc.
0002-7820,
93
, pp.
618
623
.
31.
Haanappel
,
V. A. C.
,
Shemet
,
V.
,
Gross
,
S. M.
,
Koppitz
,
Th.
,
Menzler
,
N. H.
,
Zahid
,
M.
, and
Quadakkers
,
W. J.
, 2005, “
Behavior of Various Glass-Ceramic Sealants With Ferritic Steels Under Simulated SOFC Stack Conditions
,”
J. Power Sources
0378-7753,
150
, pp.
86
100
.
32.
Ogasawara
,
K.
,
Kameda
,
H.
,
Matsuzaki
,
Y.
,
Sakurai
,
T.
,
Uehara
,
T.
,
Toji
,
A.
,
Sakai
,
N.
,
Yamaji
,
K.
,
Horita
,
T.
, and
Yokokawa
,
H.
, 2007, “
Chemical Stability of Ferritic Alloy Interconnect for SOFCs
,”
J. Electrochem. Soc.
0013-4651,
154
, pp.
B657
B663
.
33.
Tu
,
H.
, and
Stimming
,
U.
, 2004, “
Advances, Aging Mechanisms and Lifetime in Solid-Oxide Fuel Cells
,”
J. Power Sources
0378-7753,
127
, pp.
284
293
.
You do not currently have access to this content.