J. Turbomach. March 2022, 144(3): 031011.
Paper No: TURBO-21-1177
Published Online: October 18, 2021
...Nandana Menon; Tanjheel Hasan Mahdi; Amrita Basak Nickel-base superalloys are extensively used in the production of gas turbine hot-section components as they offer exceptional creep strength and superior fatigue resistance at high temperatures. Such improved properties are due to the presence...